Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_35249787524e22e49830248dd31a4d0c |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-16 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J121-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J109-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J111-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J121-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J111-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J109-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J161-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J201-00 |
filingDate |
1998-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2003-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_24e70302d26d832910ace6eb3242027c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9027df4c655bfb2dcb19d1fd1a089100 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d9ec52574856bfe89228ea9ba3b661d1 |
publicationDate |
2003-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-6635703-B1 |
titleOfInvention |
Very high solids adhesive |
abstract |
A method of making a contact adhesive includes the steps of mixing a solvent with a rubber blend and/or resin for making a contact adhesive and then processing the solvent/rubber/resin blend until a desired lowered viscosity is reached while obtaining a solids content of greater than 30 weight percent. The contact adhesive has a viscosity capable of allowing atomization of an adhesive which contains a solids content of greater than 30 weight percent. |
priorityDate |
1998-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |