abstract |
The method for manufacturing coated steel sheet has the steps of: immersing a steel sheet in a hot-dip coating bath to form an Al-Zn base coating layer containing 20 to 95 mass % Al on the steel sheet, forming a passivated layer on the coating layer; and applying thermal history to the coating layer. The thermal history is applied immediately after the steel sheet left the hot-dip coating bath or in a temperature range of from T(° C.) between 130° C. and 300° C. to 100° C. |