Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24c39e4dc286833abc38483ab3822aee |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2011-0041 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2031-757 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S425-808 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00125 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00519 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-0023 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02C7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29D11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-10 |
filingDate |
2000-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2003-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_801fb481843023fdb569de60ee5d28fd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0bd3fd9febe5e8bd7146f0f833942b9e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1467f5c9ca3f2650a2de6d0b72aeb5bd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cc527e12f913f44f90a8f66a1acc5982 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_491eaf733c890e6eada1c395537a8266 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6409d7cdfd6117fe30dfef3aacffcfd0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c45a9d7992a1b3549e5d74267622fd6a |
publicationDate |
2003-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-6610220-B1 |
titleOfInvention |
Process of manufacturing contact lenses with measured exposure to oxygen |
abstract |
This invention provides a method of manufacturing a contact lens comprising the step of: dosing a contact lens mold comprising optical mold surfaces with an oxygen-sensitive reaction mixture, wherein said optical surfaces of said contact lens mold have between from 0.13x10-9 to 2.6x10-9 moles/cm2 O2 available to interfere with the reaction of said reaction mixture. This invention further provides a method of manufacturing a contact lens comprising the steps of: dosing a contact lens mold comprising optical mold surfaces with a reaction mixture, and sealing said reaction mixture and said optical mold surfaces away from a gaseous environment, wherein said optical surfaces of said contact lens mold were exposed to said gaseous environment comprising greater than 0.5 percent oxygen just prior to said sealing step. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8070475-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11754754-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2008150178-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11187920-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10620456-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011287118-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7850878-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2008131593-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11125916-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009166507-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10209534-B2 |
priorityDate |
1998-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |