http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6565922-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_082507838ffd3a482218a2d116731fbd |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-037 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-02 |
filingDate | 2002-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2003-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_78baebf39adfecfbb80eca9036507a11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8ddea21a385db2a5379c49a8d97372fe http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0cba6abe597241bfccd1b779a159c0ab |
publicationDate | 2003-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-6565922-B2 |
titleOfInvention | Method of decorating a ceramic substrate |
abstract | The present invention provides a method of decorating a ceramic substrate. The method according to the invention includes applying a slurry that includes solid particles of at least one color-contributing metal salt dispersed in a saturated solution of at least one color-contributing metal salt having a viscosity of from about 10 to about 20,000 centipoise to a ceramic substrate, applying a solvent to the ceramic substrate in amount sufficient to at least partially dissolve the solid particles, and firing the ceramic substrate. Preferably, the solid particles in the slurry have a diameter of less than about 40 microns. The present invention also provides a porcelain tile decorated in with the method. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006163957-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9909023-B2 |
priorityDate | 2000-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 65.