Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1e70c0aeade92d7571d955d3b90ea06e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2375-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2913 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2927 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4854 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-346 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F1-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-94 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 |
filingDate |
2000-09-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2003-03-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9005f8de3ef2d03d40e8ad5829403e07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ba56b1edc04c68eedbd10ac7b25c943a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d335ea37dda37b7c1f5a0a57dbbba214 |
publicationDate |
2003-03-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-6533975-B1 |
titleOfInvention |
Process of making polyurethane fiber or film |
abstract |
This invention provides processes for preparing fiber or film comprising a polyurethane and layers delaminated from a lamellar clay, said layers being dispersed in said polyurethane. Fiber and film produced by the processes of the present invention exhibit reduced tack and an increased ability to affix at least one dye. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007009724-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2008176972-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007072991-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9345997-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100599197-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009226744-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8329286-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8524920-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8524919-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102127827-B |
priorityDate |
1996-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |