http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6454953-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d5d04736b0b882a4f5a1e0e0e4cd8cbb |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-13 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-0029 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-56 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-15 |
filingDate | 2001-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2002-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c46c1185e5d4685d1a15cb4f1668c7b4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d2c8e1b7e73fc7ea3a2955bc1aa35859 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_26dabafb09e188fef9eb7a4ee4227f6e |
publicationDate | 2002-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-6454953-B2 |
titleOfInvention | Solid electrolytic capacitor and method for producing the same |
abstract | An object of the present invention is to provide a solid electrolytic capacitor with excellent electrostatic capacitance and reduced dispersion of capabilities by treating the surface of a chemically formed aluminum film to form a dielectric film which is in contact an electrically conducting substance provided thereon with sufficiently high adhesion. Another object of the present invention is to provide a method for producing the solid electrolytic capacitor, which includes providing an organic electrically conducting polymer as a solid electrolyte on a chemically formed aluminum substrate having thereon an aluminum oxide dielectric film, where a chemically formed aluminum substrate, which was cut into a predetermined shape, is treated with an aqueous acid solution to dissolve a part of the dielectric film on the substrate surface. The present invention also provides an aluminum solid electrolytic capacitor obtained by the method, and a chemically formed aluminum substrate for aluminum solid electrolytic capacitors. |
priorityDate | 2000-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 157.