abstract |
Novel methods and devices which provide enhanced mixing and application of two liquid components to form a biomaterial with minimized aerosols is achieved using air flow rates below about 1.25 liters/minute in combination with a ratio of air flow to total liquid flow of from about 150:1 up to about 1500:1. Preferably the air flow is below about 1 liter/minute and the ratio of air flow to total liquid flow is from about 200:1 to about 1200:1. The parameters are ideally suited for the spray application of components which form a surgical sealant, e.g., a fibrin sealant. Also a part of the present invention are novel application methods for biomaterial, e.g., surgical sealant, components at liquid flows below 1.9 ml/minute, novel methods involving the mixing of such components on the exit surface of a spray tip or nozzle, novel spray tips and biomaterial applicators and methods for making such applicators. |