abstract |
A preferred OPTICAL BLACK(TM) ionic anodize process of the present invention applies a porous anodic oxide coating to a component part in a standard sulfuric acid anodizing bath (with or without organic additives). A modified alternating electric current is then applied to the porous oxide coating to remove excess anodizing electrolyte and to allow the coloring solution access to the pores. The oxide coating is electrolytically colored in a low pH acid bath containing a tin salt, sulfuric acid, and organic additives. Alternating current carries additional tin salt to the base of the pores where the tin salt is reduced to metallic tin or tin oxide. Others metals or metallic salts could be employed. Component parts treated by the OPTICAL BLACK(TM) ionic anodize process can be advantageously employed in optical systems, such as particle detectors, to reduce or eliminate stray light. |