http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6403707-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c62268de3e92657ca5b9adcac4778225 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2913 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-249921 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F287-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F287-00 |
filingDate | 2000-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2002-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a432942a9795120d71dca5bd6f914194 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_72fae6d26c77c57e458e78c8245f2944 |
publicationDate | 2002-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-6403707-B2 |
titleOfInvention | Rubber-modified styrene type copolymer |
abstract | A rubber-modified styrene type polymer comprising from 1 to 15 parts by weight of a dispersed phase made of a rubber-like elastic material and from 99 to 85 parts by weight of a continuous phase made of a polymer comprising from 35 to 75 wt % of styrene type monomer units and from 65 to 25 wt % of (meth)acrylate type monomer units, wherein the rubber-like elastic material is a styrene (30 to 50 wt %)-butadiene (70 to 50 wt %) block copolymer, the weight average molecular weight (Mw) of the polystyrene portions of this block copolymer is from 45,000 to 75,000, and the ratio (Mw/Mn) of Mw to the number-average molecular weight (Mn) is from 1.20 to 1.80. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9745625-B2 |
priorityDate | 1999-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 138.