abstract |
A polyolefin composition is provided which consists essentially of isotactic polypropylene and, optionally, one or more comonomers, wherein the total comonomer content of the polyolefin composition is from 0 to 20 mole percent, and further, wherein the weight average branching index g' for the lower molecular weight region of the polyolefin composition is less than 0.93. Additionally, a process is provided for producing a polyolefin composition comprising:a) contacting, in solution, at a temperature from about 90° C. to about 120° C., propylene monomers with a catalyst composition comprising a first chiral, stereorigid transition metal catalyst compound capable of producing isotactic polypropylene;b) copolymerizing the product of a) with propylene and, optionally, one or more copolymerizable monomers, in a polymerization reactor under suitable polypropylene polymerization conditions using a second chiral, stereorigid transition metal catalyst capable of producing isotactic polypropylene; andc) recovering a branched olefin polymer. |