http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6258909-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C69-007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F212-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C69-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C43-285 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C43-295 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C69-007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C69-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C43-295 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C43-285 |
filingDate | 1998-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2001-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_200a16a438b67457cfdb1435e4b129af |
publicationDate | 2001-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-6258909-B1 |
titleOfInvention | Polyester resins |
abstract | A polymerizable vinylester composition is described which comprises at least three monomers and oligomers, said composition comprising:2-95% by weight of:diaryl compounds comprising at least two aryl groups linked directly together or bridged by a linking group, each of said at least two aryl groups having a vinyl group attached thereto,2-65% by weight of:a methacrylic acid ester of a vinyl-substituted sec-ethylol-diaryl oxide or its thioether or methine or biphenyl counterpart, and1-35% by weight of:dimethacrylic acid esters of bis-[4-(1-hydroxyethyl)aryl] ether, thioether or methine, or their counterparts where aromatic rings are linked together directly, and2-95% by weight of:unsaturated oligomers, andsaid reactive composition has less than 1% mol basis of monoaryl phenolic compounds. A method of synthesizing polymerizable divinylaromatic compositions of the invention is described comprising the steps of dehydrating a diol by heating wherein heating said diols is performed in the presence of a sulfonic acid at a concentration of 0.5-10.0 mmole/L in aromatic solvent at the boiling temperature of the reaction mixture in the range of 100-160° C., and then removing at least some water produced by the dehydration reaction. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6594427-B1 |
priorityDate | 1998-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 220.