Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be055db3c1a09879df07379ba969e223 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2215-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2215-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2215-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2215-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2215-412 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2215-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2215-31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2215-16 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B11-086 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B11-082 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C33-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-73 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-82 |
filingDate |
1998-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2000-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_779c5477263d43cc50b7f29f171bb1d5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e3bb33286f4b701c28edd6311db4b6a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f78bc8e18a2c435657140bdbc27b375 |
publicationDate |
2000-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-6151917-A |
titleOfInvention |
Press-molding die for magnetic-disk glass substrate |
abstract |
A press-molding die can manufacture magnetic disks suitable for the zone-texture technique in large quantities and at a low price by forming smooth surface areas and rough surface areas on the surface of the press-molding die. A manufacturing method for this press-molding die is provided. A magnetic-disk glass substrate that has improved CSS properties and allows a lower flying height is formed using this press-molding die. An intermediate layer is formed by sputtering on a die base material. A mask having an aperture is formed on the intermediate layer. The surface of the intermediate layer is roughened by etching in the aperture. A first protective layer is formed by sputtering in the etched portion. After the mask has been removed, a second protective layer is formed on the intermediate layer by sputtering. The surface roughness of the rough surface portion is reflected by the surface roughness of the first protective layer. The surface roughness if the first protective layer is reflected by the surface roughness of the second protective layer. Thus, a rough surface portion can be formed on the second protective layer. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8245537-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011011732-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11534861-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013237034-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11148943-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010071416-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-101588996-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6314763-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7143609-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6314764-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004093518-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11383322-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004079114-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9981844-B2 |
priorityDate |
1997-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |