http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6024556-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_aa6e4421d9e1159b6012d9bf702be572 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f1192a135e4bc40a5f201a9646f20172 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-32 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-32 |
filingDate | 1998-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2000-02-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_54c9072a1b751a5f7063ba08a1dea6e0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4dcd7339ba577ab19b220bb7585b248f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_31a9a92bb8b6c10f106e89d4acc60cfa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fd3def4ddcdd9b20c8c28bf84fa6acbc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_655bc556108ac585dcc501989a3c9322 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6868528b42fcc09381bf86ce2b462024 |
publicationDate | 2000-02-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-6024556-A |
titleOfInvention | Spinneret for producing composite polymer fibers |
abstract | A composite polymer fiber is produced employing at least two polymer compounds according to a process for producing a composite polymer fiber including the steps of supplying at least two polymer compounds; forming a belt flow by arranging alternately unmixed strips of the polymer compounds supplied; and injecting the belt flow after it is compressed such that the thickness of the belt flow may be longer than the width thereof and that multiple layers of the polymer compounds may be parallel to the longer axis of the fiber. According to this process, there is obtained a fiber having a multilayered structure, in which the thickness of each layer can be controlled with optical accuracy since the multilayered structure is formed in one step, and also having a rectangular cross section in which each layer in the fabric is oriented parallel to the longer axis of the fiber, so that the layers can be easily oriented, when woven into a fabric, in such a direction as to obtain high-intensity coherent beams of light. |
priorityDate | 1997-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |