http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6017684-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C2001-0055 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-49827 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C8-404 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C8-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-08 |
filingDate | 1997-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2000-01-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1ebb19cc50aa1ae3f759119d19f870c1 |
publicationDate | 2000-01-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-6017684-A |
titleOfInvention | Silver halide color photographic light-sensitive material and a method of forming color images |
abstract | The present invention provides a silver halide color photographic light-sensitive material including a substrate having a photographic constituent layer coated thereon including at least one light-sensitive layer which includes a light-sensitive silver halide emulsion, a developing agent, a compound capable of forming a dye by a coupling reaction with the oxidation product of the developing agent, and a binder, the light-sensitive material after the exposure thereof being put together with a processing material including a substrate having a constituent layer coated thereon including a processing layer comprising a base and/or a base precursor, in the presence of water supplied to the light-sensitive layer of the light-sensitive material or to the processing layer of the processing material in an amount ranging from +E,fra 1/10+EE to the equivalent of an amount which is required for the maximum swelling of the entire coating layers of these materials, so that the light-sensitive layer and the processing layer face each other, and being heated for the purpose of heat development to form a color image in the light-sensitive material, in which the light-sensitive silver halide emulsion contains at least one ion selected from the group consisting of a metal ion and a metal complex ion which are each an electron trap having a depth of 0.6 eV or less, and contains at least one kind of tabular grain having an average aspect ratio ranging from 4 to 100. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6664033-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6262756-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2002198517-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7033348-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6348302-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6413704-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6531274-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6562559-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6171775-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6555302-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6610467-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004033452-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6261746-B1 |
priorityDate | 1996-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 287.