Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5d4ada69388e0a1b68daaf536597c732 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-12 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-3081 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-309 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-159 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-16 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-159 |
filingDate |
1998-02-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1999-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f6501e877c303fc1653324384e09cd26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b4873d111402865ca6b85ad82609f73b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b406f2d5a3e2116fe5b8301255a6092e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c945056fd98075dd7b019049afe87a92 |
publicationDate |
1999-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-5942590-A |
titleOfInvention |
Process for making hydrophobic silica with reduced surface area under neutral conditions |
abstract |
The present invention is hydrophobic silica gels having a reduced surface area and a method for their preparation under neutral conditions. The method comprises two steps, where in the first step the pH of a mixture comprising a silica hydrosol and colloidal silica is adjusted with a base to within a range of pH 3 to pH 6 to facilitate formation of a silica hydrogel having incorporated therein colloidal silica. In the second step the silica hydrogel is contacted with an organosilicon compound in the presence of a catalytic amount of a strong acid to effect hydrophobing of the silica hydrogel to form a hydrophobic silica gel having a surface area within a range of about 100 m 2 /g to 450 m 2 /g in the dry state. In a preferred process the hydrophobic silica gel is contacted with a sufficient quantity of a water-immiscible organic solvent to convert the hydrophobic silica hydrogel into a hydrophobic silica organogel. A water soluble compound of cerium or iron may be added during conduct of the second step to improve heat stability of the hydrophobic silica gel. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2110414-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8455165-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6579929-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9388314-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8202502-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10407571-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6051672-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009127438-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006258780-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006241222-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6596250-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011039983-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005233937-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8435474-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6852299-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8361946-B2 |
priorityDate |
1997-02-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |