Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20688220cab72ad01902ff5223732946 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C2001-03594 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-95 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-7614 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S430-162 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S430-151 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C8-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-07 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-95 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C8-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-07 |
filingDate |
1997-07-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1998-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5fff6b9e69bd1afae09746cfd6eb46da http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1f4f5ba5072de9c908b083114a64e2ab |
publicationDate |
1998-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-5795697-A |
titleOfInvention |
Imaging element for making an improved printing plate according to the silver salt diffusion transfer process |
abstract |
The present invention provides an imaging element comprising in the order given on a hydrophilic surface of a support (i) an image receiving layer containing physical development nuclei, (ii) a photosensitive layer containing a silver halide emulsion being in water permeable relationship with said image receiving layer (iii) a first antistress layer and (iv) a second antistress layer, said antistress layers being in water permeable relationship with said image receiving layer and each independently comprising unhardened gelatin, characterized in that said second antistress layer comprises at least 30 mg/m2 of a matting agent with a weight average diameter of more than 3 mu m. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6228557-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004091490-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004247588-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6300034-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6120971-A |
priorityDate |
1996-07-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |