http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5777056-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2cb72657cf0479385a9b5e655af1e16f |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F110-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-14 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F10-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F110-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-654 |
filingDate | 1996-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1998-07-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_038f07260eb2d6e91c17b46499509fcf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_98defc0552b801d37a1d42ca78866340 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_42827d049938cac521a88b06441b7175 |
publicationDate | 1998-07-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-5777056-A |
titleOfInvention | Polyolefinic resin and a resin composition comprising said resin |
abstract | A polyolefinic resin which is a homopolymer of an olefin or a copolymer of olefins, has (i) intrinsic viscosity η! measured in decaline at the temperature of 135° C. in the range of 0.5 to 10 deciliter/g and (ii) content of insoluble fraction in boiling n-heptane (W) in the range of 10 to 99 weight % and shows (iii) relation between relaxation time of rubber component measured by pulse NMR at the temperature of 30° C. T 2H R (30):μs!, relaxation time of rubber component measured by pulse NMR at the temperature of 80° C. T 2H R (80):μs! and the content of insoluble fraction in boiling n-heptane (W) satisfying the following equations: n n T.sub.2H.sup.R (80)≦670-2.2×W n n n T.sub.2H.sup.R (80)/T.sub.2H.sup.R (30)≦8.8+0.086×W n n and a propylenic resin composition comprising (A) 10 to 95 weight % of the polyolefinic resin, particularly a propylenic resin which is at least one kind selected from a homopolymer of propylene and copolymers of propylene containing 4 mol % or less of other olefinic units, and (B) 90 to 5 weight % of a propylenic random copolymer having intrinsic viscosity η! measured in decaline at the temperature of 135° C. in the range of 0.5 to 10 deciliter/g and containing 10 to 80 mol % of olefinic units other than the propylenic unit are disclosed. The polyolefinic resin and the composition have high heat resistance and excellent mechanical properties in a wide range of modulus, show small temperature dependence of the mechanical properties and do not cause stickiness on the surface of molded articles. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10619040-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005119392-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108290976-A |
priorityDate | 1992-12-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 588.