Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_31f87c170ea6e478544c388bd11bb684 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2023-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S264-29 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F1-106 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-46 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 |
filingDate |
1995-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1998-04-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_61c2821da65a14e11d401a5bd0d5fa14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_78ce62a2c665b8ca522d3143e6cc96b6 |
publicationDate |
1998-04-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-5738745-A |
titleOfInvention |
Method of improving the photostability of polypropylene compositions |
abstract |
A method of improving the effectiveness of a photostabilizer in reducing the deleterious effects of actinic radiation on a polypropylene composition, which method involves compounding a melt-extrudable thermoplastic polypropylene composition having a melt flow rate in a range of from about 18 to about 100 g/10 minutes at a temperature of 230 DEG C. and a load of 2.16 kg. The polypropylene composition includes a first thermoplastic polypropylene having a melt flow rate lower than 18 g/10 minutes at a temperature of 230 DEG C. and a load of 2.16 kg, a polydispersity greater than about 2.6, and a Z-average molecular weight greater than about 300,000; a second thermoplastic polypropylene having a melt flow rate higher than 18 g/10 minutes at a temperature of 230 DEG C. and a load of 2.16 kg, a polydispersity equal to or less than 2.6, and a Z-average molecular weight equal to or less than 300,000 as determined by gel permeation chromatography; and a photostabilizer. The weight ratio of the first polypropylene to the second polypropylene is in a range of from about 95:5 to about 10:90. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010121121-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8168839-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016053468-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011179558-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6642171-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005244619-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10766981-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005170727-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112877808-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6132839-A |
priorityDate |
1995-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |