http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5714302-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_663cad2cddb9415ae5ba8d9c99803cda |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41N3-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41N3-08 |
filingDate | 1996-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1998-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_32f915918d5081b74ac572e5da8bf9a9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_12a3274f2eb84014dfee4c72d39a74ee http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7b08d37e605f1ebc31c0b74a5aefed87 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f937b7e6e263345d1252828bd3705e17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5e4933f54f9ea3b7e6182a5854af669a |
publicationDate | 1998-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-5714302-A |
titleOfInvention | Method of printing with using lithographic printing plate made by silver complex diffusion transfer process and using dampening composition containing nonionic surface active agent |
abstract | The present invention provides a printing method using a silver salt lithographic printing plate obtained by imagewise exposing a silver salt lithographic printing plate precursor comprising a support and, provided thereon, at least a silver halide emulsion layer and a physical development nuclei layer and then subjecting the exposed printing plate precursor to silver complex diffusion transfer development and using a dampening composition containing a nonionic surface-active agent represented by the following formula [I]: <IMAGE> [I] wherein R represents an alkyl group of 1-9 carbon atoms, and n1 and n2 are mol numbers necessary for the polymer having an average molecular weight of 250 or more, and n1/n2 is 0.5-2, and a polymer represented by the following formula [II]: <IMAGE> [II] wherein m is a number which provides a number-average molecular weight of 2000-50000 for the polymer. By applying the above-mentioned dampening composition to the silver salt printing plate, a sufficiently high printing performance can be obtained without using colloidal silica or colloidal alumina in the dampening composition. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6312873-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0985546-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-100352870-C http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8065958-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6294318-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1415826-A3 |
priorityDate | 1993-01-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |