Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b5aed7bcdd19c8d990e720c02b318f48 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C11D3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-325 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-32 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C11D3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C11D3-08 |
filingDate |
1995-06-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1997-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9a47d0d7820f8fc0534d5dc6847e88dc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ab0bce985d24d82cbeb57cbfd8bfa8c3 |
publicationDate |
1997-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-5693304-A |
titleOfInvention |
Amorphous alkali metal silicate process and uses |
abstract |
A particulate amorphous alkali metal silicate is prepared by heating a mixture of silicate glass and water or aqueous solution to a temperature of about 300 DEG -400 DEG C. to provide a foamed material that is easily formed into particles of less than 20 microns. After careful hydration, a product having 1-15% water based on loss of ignition (LOI) of product at 800 DEG C. is produced that controls the activity of magnesium in solutions and is, therefore, a useful detergent ingredient. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5807529-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6541443-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6329335-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7449125-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005279963-A1 |
priorityDate |
1993-08-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |