abstract |
Thermoplastic moulding materials containing A. 15 to 80 parts by weight of a thermoplastic polycarbonate or polyester carbonate, and B. 4 to 40 parts by weight of a graft polymer of B.1 20 to 60 weight % of one or more monomers on B.2 40 to 80 weight % of one or more graft bases having glass transition temperatures <0 DEG C., and C. 16 to 45 parts by weight of a thermoplastic, aromatic vinyl (co)polymer, wherein the graft base B.2 has an average particle size (d50 value) of 0.20 to 0.35 mu m and the weight ratio of components B:C is between 2:1 and 1:4. |