http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5637433-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08797 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08795 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-0821 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08708 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 |
filingDate | 1996-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1997-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_324cad1499d95a13985ffed4b06a0fda http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5539e174e5296447b980e00733a99155 |
publicationDate | 1997-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-5637433-A |
titleOfInvention | Toner for developing an electrostatic latent image |
abstract | Disclosed is a toner for developing an electrostatic latent image, comprising a binder resin, a colorant and a releasing agent, wherein said toner has: (1) a storage modulus (G') having a falling starting temperature of 45 DEG to 65 DEG C., when a visco-modulus of said toner is measured by a rheometer, (2) a first inclination represented by (+E,fra 1/3+EE )x(log ( eta '121)-log ( eta '118)) is -0.065 to -0.035 at 120 DEG C. wherein said log ( eta '121) represents a common logarithm of a fusion viscosity ( eta +E,gra +EE ) of said toner at 121 DEG C., said log ( eta '118) represents a common logarithm of a fusion viscosity ( eta +E,gra +EE ) of said toner at 118 DEG C., and said first inclination represented by (+E,fra 1/3+EE )x(log ( eta '121)-log ( eta '118)) represents an inclination of a tangent at 120 DEG C., when said logarithm of said fusion viscosity ( eta +E,gra +EE ) is plotted as a function of degree of Celsius, and (3) a second inclination represented by (+E,fra 1/3+EE )x(log (G'200)-log (G'197)) is not less than -0.025 at 200 DEG C., wherein said log (G'200) represents a common logarithm of said storage modulus (G') at 200 DEG C., said log (G'197) represents a common logarithm of said storage modulus (G') at 197 DEG C., and said second inclination represented by (+E,fra 1/3+EE )x(log (G'200)-log (G'197)) represents an inclination of a tangent at 200 DEG C., when said logarithm of said storage modulus (G') is plotted as a function of degree of Celsius. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6329114-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5968701-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6040104-A |
priorityDate | 1995-07-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 84.