Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1af8df51ce24ca931ae718fb747f6aa0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-82 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-74 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-09708 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-097 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G19-02 |
filingDate |
1995-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1997-03-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7c545dc781a28abb2e1bc25017472306 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_97aaddc8840112526e05b37577d87f0f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_22c7f913af8196a4e8ba135cb8135e32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3ebca399a72e9481c01587eb8ec6df0e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5896e7d9b66a0cedbe0e855aecb32491 |
publicationDate |
1997-03-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-5614344-A |
titleOfInvention |
Toner for developing electrostatic images and image forming method |
abstract |
A toner for developing electrostatic images contains toner particles containing at least a binder resin and a colorant as well as a fine powder comprised of base particles on which crystalline low resistance tin oxide films are formed. The crystalline low resistance tin oxide contains less than 100 ppm of antimony, arsenic and phosphorus, and has an oxygen deficiency structure. The toner is excellent in strength and can consistently give high quality images under any environmental conditions. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007005823-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2008209088-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011131353-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8966144-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6569589-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6594462-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5783345-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8504746-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9189437-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006288148-A1 |
priorityDate |
1994-06-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |