http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5439946-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e83d93ed02bbd6159e99b5a7796e3686 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F222-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-02 |
filingDate | 1992-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1995-08-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_23c7668068080b57ed6ecb2653b8fcb4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_91f4f4030a921a4957cc9c78bc1471e8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_69586114965c4eafffea719b58b140be |
publicationDate | 1995-08-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-5439946-A |
titleOfInvention | Process for preparing intrinsically foamed thermoplastic polymer |
abstract | PCT No. PCT/NL92/00040 Sec. 371 Date Aug. 30, 1993 Sec. 102(e) Date Nov. 1, 1993 PCT Filed Feb. 27, 1992 PCT Pub. No. WO92/15638 PCT Pub. Date Sep. 17, 1992.Process and intermediate for preparing an intrinsically foamed thermoplastic polymer comprising a vinyl monomer and maleic acid and/or maleic anhydride, in which process a polymer composition comprising: a) a core polymer based on a.1) 12-50 moles % maleic acid and/or maleic anhydride a.2) a vinyl monomer, and a.3) optionally a third monomer, where the sum total of a1+a2+a3 is 100 moles % and the weight average molecular weight of the core polymer is 50000-500000, and b) optionally a nucleating agent, is introduced into equipment suited for making foam, in which process the core polymer, and optionally the nucleating agent, are brought to a temperature which is high enough to release CO2 from the core polymer, and in which process the polymer melt is expanded to form a polymer foam with the desired density. The core polymer is preferably a polymer of styrene and maleic anhydride. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2008286551-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5736253-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6515056-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011098372-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2010000572-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8221663-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009181207-A1 |
priorityDate | 1991-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links