Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c72d118f5664072de841f9c5c34b9d99 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-527 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K23-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-49 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-527 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C47-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 |
filingDate |
1993-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1995-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2a86f522eaff418c40cd123d12ad60d4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c510dd2838cad0a349071f7e93178c97 |
publicationDate |
1995-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-5414034-A |
titleOfInvention |
Processing stabilizer formulations |
abstract |
Melt extrusion processes involving phosphite stabilized polyolefin compositions subject to solid by-product formation during melt extrusion are improved by the addition of a metal salt of a lactic acid to the composition. The processes involving the improved compositions exhibit reduced levels of screen pack plugging during fiber and film extrusion processes than that achieved with fatty acid salts, such as calcium stearate. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015090671-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6172153-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5574082-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6077890-A |
priorityDate |
1993-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |