abstract |
PCT No. PCT/JP88/00585 Sec. 371 Date Feb. 15, 1989 Sec. 102(e) Date Feb. 15, 1989 PCT Filed Jun. 16, 1988 PCT Pub. No. WO88/10233 PCT Pub. Date Dec. 29, 1988.Fine and homogeneous oxide particles for superconductors which can be sintered at a low temperature are prepared in a liquid phase by the sol-gel method using alkoxides as starting materials. By forming a buffer layer between a substrate and a superconducting film, good-quality and oriented superconducting film can be fabricated. Highly c-axis-oriented superconducting film and bulk products can be prepared from particular starting compositions in Ln-Ae-Cu-O and Bi-Ae-Cu-O systems. The oriented film can be produced by painting a paste of such starting compositions on a substrate followed by sintering, and the bulk form can be produced by pressing the pre-sintered powder of such starting compositions. |