abstract |
PCT No. PCT/JP91/00332 Sec. 371 Date Nov. 5, 1991 Sec. 102(e) Date Nov. 5, 1991 PCT Filed Mar. 12, 1991 PCT Pub. No. WO91/13937 PCT Pub. Date Sep. 19, 1991.A flame retardant resin composition comprising (A) 70 to 10% by weight of a rubber-reinforced styrene base resin, (B) 20 to 85% by weight of a polycarbonate resin, (C) 5 to 35% by weight of a high molecular weight halogen-containing compound of the formula: <IMAGE> (I) <IMAGE> wherein n is an average polymerization degree and an integer of 4 to 30, R and R' are independently a hydrogen atom, a methyl group, an epoxypropyl group, a phenyl group, a halogenated phenyl group or a group of the formula: <IMAGE> wherein m is an integer of 0 to 3, which compound has a bromine content of at least 45% by weight and an epoxy equivalent of at least 10,000 g/mol, and (D) 0 to 10% by weight of an antimony compound, which resin composition is excellent not only in heat stability but also in heat resistance, impact resistance, processability and light resistance. |