http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5198327-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S430-164 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S430-167 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C5-29 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-29 |
filingDate | 1991-12-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1993-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fe3a576c0e959eddff9a7050afc63d64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c70727fa39a0cdd352e031da2f923c71 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_529d9a4e457dd62853f2add3f53e0c79 |
publicationDate | 1993-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-5198327-A |
titleOfInvention | Method of formation of photographic images |
abstract | For formation of a photographic image by development of a silver halide photographic material with an automatic developing machine, a certain period of time or not longer than 15 seconds is set as the time of the development step and a silver halide photographic material is used which, when developed for a period of one-half of said certain period of time after such an exposure that the exposed silver halide photographic material, when developed for said certain period of time, would give a value of (Dmax-fog)x1/2, gives a value of (D-fog) having 70% or more of the value of (Dmax-fog)x1/2. The silver halide photographic material comprises at least one of a combination of (1), (2) and (3) or (2) and (4): where: (1) represents a silver halide emulsion containing a water-soluble iridium salt; (2) represents a silver halide emulsion layer with a silver amount from 1 to 3.5 grams/m2 coated on one surface of said emulsion layer; (3) represents silver halide grains wherein the mean grain size is 1.0 mu or less; and (4) represents tabular silver halide grains having an aspect ratio of 4 or more. By the rapid development procedure, a sharp image with no development unevenness (drag streaks) can be obtained and the automatic developing machine to be used may be made small-sized and compact. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007157646-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-H1547-H http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6713242-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1331515-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6350562-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8047752-B2 |
priorityDate | 1987-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 114.