http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5194537-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_114e4423ec77cbc8dab9d0a98909704e |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F20-42 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-00 |
filingDate | 1990-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1993-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5a5e5fefb7dc0fbdfeebd1d1325a8fc6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3db20d0181896628de4bdbdbc92418e6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_99eb02ebf41af462f752a0b30b95f617 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2b4bfca8cebec0d18e5e06354e2ffa8f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_675cc47fa747da353650a20d7e542cf1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_75c482b89ff6123d32e1f23404fa97af |
publicationDate | 1993-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-5194537-A |
titleOfInvention | Process for the preparation of nitrile group containing polymers |
abstract | An improved process is disclosed for the preparation of nitrile group containing polymers which comprises reacting a nitrile group containing vinyl monomer with an initiator of the general formula [ArCR 1 R 2 ]⊖[N(R 3 R 4 R 5 R 6 )]⊕ wherein Ar=phenyl, substituted phenyl or a heterocyclic compound, R 1 =R 2 =H, ester, cyano, alkyl, aryl, 1,3-oxazoline, N,N-dimethyl amide and other similar alpha activating groups, or combination of them, or one of R 1 or R 2 together with Ar, where Ar is phenyl or substituted phenyl, is a nitrogen atom containing heterocyclic compound and the other being a nitrile group, R 3 , R 4 , R 5 and R 6 may be same or different and represent substituted alkyl, cycloalkyl, arylalkyl or aryl or two of the R 3 , R 4 , R 5 and R 6 together with nitrogen atom form a heterocycle with the condition that the sum of all carbon atoms or all R 3 , R 4 , R 5 and R 6 is from 12 to 50 and no more than one of the R 3 , R 4 , R 5 and R 6 is an aryl derivative in an inert atmosphere at a temperature not exceeding 60° C. Polymers with molecular weights in the range of 500 to 25,000 can be prepared. Of these polyacrylonitrile, polymethacrylonitrile and the like are known to be very useful and have diverse commercial applications. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013317188-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012139822-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6620846-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2020031897-A1 |
priorityDate | 1990-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 85.