Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c0f8dc752059a228fada0efdcc2901b9 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2995 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2383-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2998 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C43-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-244 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K19-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C43-02 |
filingDate |
1991-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1992-11-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f61743d496279e4b5531560a4dfc4b1a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_60b118c6fdebb6c07b9b1545cdde1805 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_70e16127985f4855b9404bfafb4e17c5 |
publicationDate |
1992-11-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-5160670-A |
titleOfInvention |
Method of manufacturing silicone rubber moldings |
abstract |
A method for the manufacture of silicone rubber moldings comprises the preparation of a silicone rubber composition by blending an organoperoxide having an activation energy of 25 to 41 kcal/mol into a semicurable organopolysiloxane composition whose main component is organopolysiloxane having organoperoxide-crosslinkable functional groups. The silicone rubber composition is made into a particulate form and heated at a temperature below 100 degrees Centigrade to produce a semicured, particulate molding material which retains the activity of the organoperoxide and which contains residual crosslinkable functional group on the organopolysiloxane. Subsequently a mold is filled with the molding material and the mold material is completely cured at a temperature of at least 100 degrees Centigrade under the application of pressure. The method is particularly useful for automatic molding methods. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11530305-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5595695-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2018291155-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107531997-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5904885-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/ES-2119649-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011008557-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6011105-A |
priorityDate |
1990-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |