Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8b9b07baa39efdd68eb1506a375245f8 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S264-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S264-15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S264-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S264-07 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-228 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C44-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C44-3402 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C44-3461 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C44-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C44-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C44-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-228 |
filingDate |
1990-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1992-05-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c996de9d675ef81b28238bbd1af6b3c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_820fa837d842176e65d99298fe1495e4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e2c20bc995073bc241abc77c63ea0f7e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_732d95903049db1afcd24950fee782ec http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f2091d704268c8aa95c3eeb795f6b931 |
publicationDate |
1992-05-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-5110836-A |
titleOfInvention |
Time-efficient process for making expanded polymeric products with multipass expansion of polystyrene bead |
abstract |
A method for making low density (0.8-1.1 lb/cu.ft.) expanded polymeric products uses blowing agent in an amount of only from 2 to 4.4 weight percent and aging periods of from 1 to 80 hours after each expansion step. The process uses 2 to 5 expansion steps and a polymer having a particular polydispersity, weight average molecular weight and Mz:Mn, this polymer having a greater expandability than conventional polymers. The process requires only about half of the amount of blowing agent currently being used in commerically viable processes for making expanded polystyrene products. The process can be used with or without a molding step. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6093781-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5288740-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7244380-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005238866-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2008200573-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2002117769-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5385698-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9309384-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009104663-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5703135-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5240657-A |
priorityDate |
1990-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |