Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f19621512f80f5481104f1fa1aaeb415 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-025 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-06 |
filingDate |
1990-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1992-03-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f55a3a97bac6bf20fa99850f528de6f4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_98425d10a0ebc62e4e8e07ce33a554d6 |
publicationDate |
1992-03-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-5093423-A |
titleOfInvention |
Method of making SBR thermoplastic elastomers |
abstract |
A method of making a thermoplastic elastomer composition produced by dynamic vulcanization of SBR as a dispersed phase of cross linked SBR, and a co-continuous matrix of SEBS and polypropylene. The dynamic vulcanization step takes place under conditions of shear and temperature to reach the decomposition point of crosslinked SBR, at which time the crosslinking reaction is quenched. Compositions of superior properties are achieved using this method. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6308847-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-2730242-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9181419-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004077799-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5491196-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004077792-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0807128-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006141882-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0807128-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7067582-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6284840-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2023304610-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2021356056-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6762244-B2 |
priorityDate |
1990-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |