http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5091424-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_af99df08b153738cd418446a75d09bfc |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J41-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J41-05 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J41-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J41-14 |
filingDate | 1990-07-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1992-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d8ce063c4b4c28718e9f346d07404092 |
publicationDate | 1992-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-5091424-A |
titleOfInvention | Reduction of leachables from type II anion exchange resins |
abstract | A process for reducing decomposition products released during use or storage from a strong base, Type II anion exchange resin in the hydroxide form by reacting either the chloride form or the sulfate form of the resin with a bisulfite salt before conversion of the resin to the hydroxide form, and the resin prepared from the process. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5308496-A |
priorityDate | 1989-01-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 74.