http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5086019-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c5ae7ebd37838d2a3bfc39bd5a8213f1 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-652 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B28B7-344 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B28B7-342 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B28B7-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-65 |
filingDate | 1990-02-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1992-02-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_898ea2d2e7131082d1ba4e1babcd413f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5c2521a138d7d081778dd73bfe0d55c7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9049a43c2ee31ca90875e81beb8eff40 |
publicationDate | 1992-02-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-5086019-A |
titleOfInvention | Reservoir feed method of making ceramic composite structures and structures made thereby |
abstract | A method for producing a self-supporting ceramic composite structure comprising a ceramic matrix embedding a filler, includes oxidizing a parent metal to form a polycrystalline material comprising the oxidation reaction product of the parent metal and, optionally, one or more metallic constituents. The method includes heating the parent metal to provide a source of molten parent metal and a reservoir of molten metal which is in communication with the parent metal and contacting the molten parent metal with a permeable bedding of filler. The molten parent metal reacts with the oxidant to form the oxidation reaction product and is replenished by the reservoir as the reacting continues for a time sufficient to grow the oxidation reaction product to a desired extent and thereby embed at least a portion of the bedding of filler within the oxidation reaction product to form the ceramic composite structure. The bedding of filler may have any suitable shape, including that of a hollow body, the interior of which is contacted by the molten parent metal to grow the oxidation reaction product through the shaped, hollow body of filler. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012099824-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012099824-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004224143-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9890439-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5262203-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10182471-B2 |
priorityDate | 1986-09-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 59.