Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f43c745e40c8f4a189ddad855d25cc5a |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01N25-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01N59-26 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01N25-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01N25-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01N25-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01N59-26 |
filingDate |
1989-10-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1991-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dc4c833d116b966a13aef739efe854dd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14d3a96121c3c4442583948a1b33bdbb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b42c0785a02d703265f96322fd1fc861 |
publicationDate |
1991-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-5017376-A |
titleOfInvention |
Delayed hydrolysis of metal phosphides |
abstract |
A method of producing an alkaline earth or alkaline earth metal phosphide-based hydrogen phosphide generating pest control agent by completely coating even surfaced bodies of the alkaline earth or alkaline earth metal phosphide with a moisture-permeable coating which delays the generation of the hydrogen phosphide therefrom for a desired period of several hours up to one month and which is formed from moisture-pervious, solid, organic materials. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5416029-A |
priorityDate |
1987-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |