abstract |
A method of making large particle size, high purity, dense silica is described. Tetraethylorthosilicate ethanol solution is added to a 2N ammonium hydroxide solution containing silicic acid having an average particle size of about 15 micrometers to form a precipitate followed by a digestion of the precipitate in the solution. The precipitate is filtered through a screen having 45 micrometer openings and dried to form a dried powder. The dried powder is then calcined in an oxygen atmosphere followed by densifying it by heating at a temperature of about 1200° C. in air to form a large particle size, high purity, dense silica. |