abstract |
Impact-resistant nylon molding materials contain A: a linear, thermoplastic nylon composed of radicals derived from terephthalic acid and isophthalic acid and alkanediamines of 4 to 10 carbon atoms, and B: from 50 to 60% by weight, based on A, of one or more copolymers of 1. from 50 to 80% by weight of ethylene, from 20 to 50% by weight of a primary or secondary C2-C8-alkyl ester of (meth)acrylic acid, and from 0.5 to 10% by weight of a monomer possessing an acidic functional group or a latent acidic functional group, or 2. from 70 to 98% by weight of a primary or secondary C2-C8-alkyl ester of (meth)acrylic acid, from 1 to 30% by weight of a monomer possessing an acidic functional group or a latent acidic functional group, and from 1 to 5% by weight of a monomer containing 2 or more olefinic double bonds in the molecule, the percentages stated in 1. and 2. summing to 100% in each case, and C: if required, effective amounts of additives. |