Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_66506d6dd2a9c50fa36fb8b2e55151af |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C21D9-0093 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16B33-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16B33-008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16B25-103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C28-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16B25-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21D9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C28-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16B33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16B33-06 |
filingDate |
1987-12-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1988-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4659bf19fd9a3665afb969503e06ceb6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df1a22ee0252ab08964388a77b929a7a |
publicationDate |
1988-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-4773111-A |
titleOfInvention |
Selectively hardened self drilling fasteners and process for making the same |
abstract |
A process for making self-threading screw fasteners wherein only the cutting portions of the tip of the fasteners are hardened. The unhardened portions of the fastener remain ductile and are not subject to hydrogen embrittlement during subsequent plating to improve corrosion resistance. The process preferably comprises applying a radiation curable plastic coating over the drill tip followed by plating of a thin (minimum 0.0005 inch, 0.013 mm) layer of copper. The cured coating is then removed leaving an unplated tip. The screw is then subjected to a hardening process, wherein only the portions of the screw without the copper layer are hardened. The screw may then be plated conventionally with a corrosion resistant metal. The invention is further directed to the product of the process. A second embodiment for making screws suitable for extreme corrosion resistance is also described. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5755542-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005235779-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004006860-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8074348-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/AU-719616-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004037073-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2482942-C2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7070376-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102014006885-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7377019-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6964496-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0987452-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2013055583-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007271761-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009183546-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7836745-B2 |
priorityDate |
1986-11-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |