http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4743643-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0e77f06144be4708a6ae75bd9fee56a4 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D151-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F283-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D151-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-08 |
filingDate | 1986-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1988-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f7d0d1e96171c65a8dd146535a92921a |
publicationDate | 1988-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-4743643-A |
titleOfInvention | Dispersion of addition (co)polymers in an organic liquid |
abstract | Stable dispersion of addition (co)polymers in an inert relatively non-polar organic hydrocarbon liquid, the dispersed particles embracing both a (co)polymer and a polymer containing an ethylenically unsturated monamer. The (co)polymers are substantially composed of: (a) 5 to 100 mole % of styrene and/or methyl styrene; (b) 0 to 95 mole % of alkyl methacrylate having 1 or 2 carbon atoms in the alkyl group and/or alkoxyalkylene methacrylate having 1 or 2 carbon atoms in the alkoxy group and the alkylene group; (c) 0 to 40 mole % of alkyl methacrylate having 3 to 12 carbon atoms in the alkyl group; (d) 0 to 40 mole % of hydroxyalkyl methacrylate having 2 to 12 carbon atoms in the alkyl group and/or glycidyl methacrylate; and (e) 0 to 20 mole % of methacrylic acid. The (co)polymers are grafted to a polymer of a number average molecular weight of 2,000 to 10,000, at least 60% by weight of which consists of butadiene, the weight percentage of the butadiene-containing polymer being 20 to 200% of that of the (co)polymer and the sum of this percentage and the percentage of styrene and/or methyl styrene in the copolymer being higher than or equal to 50. At room temperature the dispersions dry to form a smooth and very glossy film. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6652961-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5362806-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5733973-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013165586-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8822600-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6165457-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4857574-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6511740-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5777001-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5807518-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5929173-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0778298-A3 |
priorityDate | 1984-07-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 170.