Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1e70c0aeade92d7571d955d3b90ea06e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2933 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2927 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2962 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2969 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2913 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M11-79 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M11-79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 |
filingDate |
1987-03-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1988-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6d4e783b30a533ffcfdf287a36c1b694 |
publicationDate |
1988-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-4722864-A |
titleOfInvention |
Heat-strengthened yarn |
abstract |
Application of hydrophobic silica to an anisotropic-melt forming polyester yarn reduces interfilament and intrafilament fusion during heat-strengthening. Improvements in adhesion of yarn to certain matrices are noted. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5093197-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5230949-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5405697-A |
priorityDate |
1985-06-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |