Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_42206fe75eab96a992861f84398e420e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S359-90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S522-905 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B6-3801 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B6-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B6-4204 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F299-065 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F299-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B6-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B6-38 |
filingDate |
1983-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1986-09-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8248c03d0758880d739bfd3bebd863f4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b290f2b79d11d4abb7868a8605547fa |
publicationDate |
1986-09-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-4610746-A |
titleOfInvention |
Method of optically connecting a light conductor to an electro-optical device |
abstract |
In the optical connection of telecommuniation glass fibres to semiconductors a curable composition is used which comprises a polyester urethane acrylate or a polyether urethane acrylate. The composition furthermore comprises a heat- or light-activatable initiator. n The refractive index of the cured connecting material is adjusted by the addition of both a reactive diluent which increases the refractive index and a reactive diluent which decreases the refractive index. Said reactive diluents furthermore serve to establish the desired mechanical properties of the connecting material prior to and after curing. n The curable composition is provided on the glass fibres and/or on the semiconductor laser, after which they are contacted with each other and are optically aligned. The composition is then cured by raising the temperature or by exposure to light. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6449413-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5216805-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8044474-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5178319-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5881194-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5128386-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6122428-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1134605-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1134605-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-RE35069-E http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4790620-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4793688-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4711521-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4784454-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007274636-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7156285-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4845052-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004118817-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5578156-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4995687-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4942112-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4979791-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4863536-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6542669-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5098803-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5228101-A |
priorityDate |
1983-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |