Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_600db5b93a54999d3db277d10725d525 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-246 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-24 |
filingDate |
1984-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1986-05-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_beca56b076060d024bfebbbb655d1185 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_553259f4fdeb0508823710daa877d8f0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e87ada15986343019587b53d66abde9b |
publicationDate |
1986-05-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-4588448-A |
titleOfInvention |
Process for sealing anodically oxidized aluminium or aluminium alloy surfaces |
abstract |
A process for sealing an oxidized aluminium or aluminium alloy surface comprising sealing the surface in the presence of a sealing agent to hinder the formation of a smut layer, the agent being the reaction product of one or more sulphonated aromatic compounds with an aldehyde and/or dimethylolurea or a mixture of formaldehyde and urea. A novel composition comprising the reaction product above and a cobalt or nickel salt may also be used as the above mentioned sealing agent. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0814183-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6197451-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6383307-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5374455-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5362317-A |
priorityDate |
1981-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |