Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_97f8939cf76e68731c5704c708ac7a89 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S525-902 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F265-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-12 |
filingDate |
1984-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1985-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14251f8a943f159477eecf38b6d2af52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4636d3ed268fac43437636e7d7d3ef2b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c4f91211c16ba1606a5ff7fa638d11c3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7a6ca5ea95e42c1f143c5e364d26bdce http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7be74d6bacada56acff5b55cf7c9ec95 |
publicationDate |
1985-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-4521567-A |
titleOfInvention |
Method for making impact resistant molding compositions |
abstract |
A method for making impact resistant molding compositions wherein a hard phase having a glass transition temperature above 25 DEG C. and consisting principally of methyl methacrylate is polymerized at least partially in a first stage, following which the monomers of a rubbery phase whose polymers have a glass transition temperature below 25 DEG C. are added in a second stage and the polymerization is carried to completion, polymerization of the hard phase in the first stage being performed in a presence of an oil soluble free radical initiator and of an organosulfur chain transfer agent having at least two thiol groups in the molecule, and polymerization of the monomers of the rubbery phase in the second stage being carried out with graft crosslinkers in the presence of the previously formed hard phase. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2002173589-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8426986-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5280073-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1258501-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5006593-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102575081-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102575081-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I483984-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5102939-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102010028186-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7056984-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8759450-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4737533-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1258501-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011003219-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20120095339-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5198500-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101627391-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5155172-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006058458-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011210454-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7784161-B2 |
priorityDate |
1983-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |