abstract |
An oxidation catalyst comprising boron phosphate impregnated with from 5 to 20 weight percent silver and its use to oxidize propylene, butene-1, butadiene-1,3 and methanol is disclosed. The oxidation takes place at from 200° to 700° C. Preferably water vapor is present. |