Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_af99df08b153738cd418446a75d09bfc |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-092 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-46 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-092 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-46 |
filingDate |
1982-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1983-10-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ffa790d99a4af7a0bbf16378aea42162 |
publicationDate |
1983-10-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-4407991-A |
titleOfInvention |
Oxalic acid stabilized thermosettable vinyl ester resins |
abstract |
Oxalic acid, alone or in combination with phenothiazine or with phenothiazine and 4-chloro-2-nitrophenol, increases the storage life of vinyl ester resins or unsaturated polyesters without adversely suppressing the exotherm or affecting their curability. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5034437-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5861466-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5973042-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004143051-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2097369-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5326795-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5298543-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6040396-A |
priorityDate |
1981-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |