Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5d4ada69388e0a1b68daaf536597c732 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B3-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 |
filingDate |
1979-03-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1981-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cf4622c3e75809f610c78a4315c879ca http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d62fdd8d556d16576a1023531e171ac7 |
publicationDate |
1981-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-4248768-A |
titleOfInvention |
Siloxane elastomers containing manganous oxide |
abstract |
Siloxane compositions comprising 100 parts by weight of polydiorganosiloxane, 10 to 100 parts by weight of reinforcing silica filler, and 0.1 to 5 parts by weight of manganous oxide are elastomeric bases. When further compounded with organic peroxide and optional additives and cured, the finished products exhibit improved heat stability. If flame-retardant additives are used, the finished products exhibit improved flame-retardancy. The manganous oxide is a purified material having a maximum particle size of 15 micrometers. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4504621-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4366278-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5256486-A |
priorityDate |
1979-03-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |