http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4192927-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c7ad58d3c0b071069a8ee0cb8c8ba2e8 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-3889 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4684 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-836 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-797 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-509 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-83 |
filingDate | 1979-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1980-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6152d57ca7a8e2231698bf950671ff4c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ffe8f7e8f15b4cde815901b5c0007eb6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8bbba89a5239ea99c3c712f1046ddda2 |
publicationDate | 1980-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-4192927-A |
titleOfInvention | Polyhydroxyl compounds containing phosphonormamidine groups |
abstract | The present invention relates to new polyols modified by phosphonoformamidine groups, to a process for the preparation thereof and the use thereof as starting component for the preparation of preferably foamed polyurethane plastics. n The process involves (A) reacting diisocyanatocarbodiimides corresponding to the following general formula: n n OCN--R.sup.2 --N═C═N).sub.m R.sup.2 --NCO n n at a temperature of from about 25 to 130° C., optionally in the presence of an inert solvent, with polyhydroxyl compounds corresponding to the following general formula: n n A--OH).sub.n n n in an OH/NCO-ratio of from 1.2:1 to 30:1 to form a polyhydroxyl compound containing carbodiimide groups and (B) completely or partially reacting the carbodiimide groups remaining in the product of step (A) by means of a basic catalyst at a temperature of from 25 to 150° C., optionally in the presence of an inert solvent, with a phosphite corresponding to the following general formula: ##STR1## to form phosphonoformamidine groups, and (C) distilling off the inert solvent, if used; wherein n m represents a number of from 1 to 10, and n R 1 represents a C 1 -C 18 aliphatic, C 4 -C 15 cycloaliphatic or C 6 -C 15 aromatic or araliphatic radical which may optionally contain a double bond and/or be branched and which may optionally be substituted by a group selected from the group of hydroxyl or trifluoromethyl groups, fluorine, chlorine, bromine or iodine; n R 2 represents a divalent aliphatic, cycloaliphatic, aromatic or araliphatic radical having from 4 to 25 carbon atoms obtained by removing the isocyanate groups from a diisocyanate; n A represents an n-valent radical of the type obtained by removing the hydroxyl groups from a polyhydroxyl compound having a molecular weight of from 62 to 6000; and n n represents an integer of from 2 to 8. |
priorityDate | 1977-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |