http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4144360-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4ddcb273a108a5d8472b335280098e06 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-1841 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-1889 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-208 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-52 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C17-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-51 |
filingDate | 1977-08-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1979-03-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_541339598128cb7377ec00d834d8e849 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_72f59fa29690f50c676931aac86791a9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86e8b93cf1db3da61c0930246af45706 |
publicationDate | 1979-03-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-4144360-A |
titleOfInvention | Method for the currentless catalytic precipitation of aluminum |
abstract | The invention relates to a method for the currentless catalytic precipitation of aluminum. The surface of insulating and conductive materials (substrates) to be aluminized is (1) catalyzed, while a film-forming moisture-insensitive layer is developed, with a compound active at the boundary surfaces, by a brief immersion in a dilute solution of (a) a modified ester or acylate of titanium, zirconium or vanadium, substituted at the metal atom with short- and long-chain organic radicals or (b), a chloride of the transition metals of the IV and V secondary group of the periodic system of the elements and a water-containing metal soap of a polyvalent metal, preferably aluminum soaps; (2) is intensively rinsed with aprotic solvents, preferably having a boiling point of over 100 DEG C.; and (3) is immersed in a 1 to 4% solution of trialkylaminalanes in a solvent mixture of aromatic and highly viscous aliphatic compounds. A homogeneous and strongly adhering aluminum coating is thereby obtained. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4764442-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/GB-2248853-A |
priorityDate | 1976-08-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 62.