Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7b94d2715cda37c1f23e48f9f4f23422 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T29-49076 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K1-165 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2924-0002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2924-09701 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K3-4053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K2203-0235 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T29-4902 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K1-0306 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-486 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K3-4614 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L23-5384 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K3-4629 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F41-02 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K1-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K1-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K3-40 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01F41-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L21-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L23-538 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K3-46 |
filingDate |
1977-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1978-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c51da6bc52637001e3c7e054029def9d |
publicationDate |
1978-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-4117588-A |
titleOfInvention |
Method of manufacturing three dimensional integrated circuits |
abstract |
A method of manufacturing three dimensional integrated circuits from compatible co-fireable materials by extruding batched co-fireable materials to form blocks of specified cross-sections, selecting and stacking cross-section of various widths from different blocks in a specified manner to form the desired circuit and placing the stack in a furnace having a predetermined temperature time profile to properly sinter each of the materials. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6255932-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5670824-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2017256346-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4758808-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4522671-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5532667-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4716649-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5257000-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4342143-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5576680-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6262650-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6249205-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-8001220-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11277067-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4301580-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4833568-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0865048-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5861790-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6534842-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10117334-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6817085-B2 |
priorityDate |
1977-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |