Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3492a7406879265b1f567f37d98dbbaf |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S264-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2361-06 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-143 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-10 |
filingDate |
1976-06-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1978-08-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9dbda1027cf08a79333c80c58b2c5f0e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8af631aaed724003733cb5161e23079e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_66f5d2376f5c80585df617d0cea962c3 |
publicationDate |
1978-08-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-4107107-A |
titleOfInvention |
Process for the manufacture of a flame resistant, insulating, energy-absorbing, porous phenolic foam |
abstract |
A high compressive strength phenolic resin foam is made by: adding between about 0.5 to 5.0 parts of a dual surfactant system and about 8 to 25 parts of a blowing agent, to 200 parts of a phenolic resole resin to form a pre-mix; agitating this pre-mix with about 20 to 70 parts of an aqueous dual sulfuric-phosphoric acid solution to provide a foaming phenolic material; immediately thereafter pouring or injecting the material into a mold or onto a suitable substrate, to provide a phenolic foam having a substantially uniform compressive strength of at least 40 psi. at between about 20% to 50% compression, at a deflection rate of between about 2 in./min. to about 5 in./min. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4478958-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017136878-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7318499-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4219623-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4417004-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4539338-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005183903-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4423163-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005261387-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5670101-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108779283-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4444912-A |
priorityDate |
1976-06-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |